Buying Guides

Wetsuit Repair Guide: How to Fix Tears, Seams and Zips

Which rental-suit damage a dive shop can fix in-house, how to patch a neoprene tear and a split seam, how to keep zips working, and when a suit is beyond repair.

3mm FLEX Hooded Front-Zip Diving Wetsuit

Why rental suits fail where they do

A rental wetsuit does not wear out evenly. It fails in the same places every time: the knees, the shoulders, the crotch, and the zip.
Knees wear from kneeling on boats and rocks. Shoulders and crotch wear because the seams there stretch every time a diver puts the suit on. Zips fail because sand gets into the teeth and divers force the slider when the suit is tight.
Small damage left alone becomes a dead suit. A 2 cm tear becomes a 10 cm tear after a few more dives. A seam that has started to split lets water in, and a cold diver blames the suit, not the seam. Checking suits when they come back from a dive, before they go back on the rack, is what keeps a fleet alive.

What you can fix in-house, and what to send out

Not every repair belongs in the shop. The split is simple.
Fix in-house:
  • Small neoprene tears and holes. A clean cut or tear up to a few centimetres long, away from a seam, including fingernail tears and punctures from fins and buckles.
  • Worn knee patches. A patch glued over a thin knee before it tears through.
  • Zip care. Cleaning, lubricating, and freeing a stuck slider.
Send out to a repair shop:
  • Split seams. Re-stitching a blind-stitched seam needs the right needle and machine. A hand stitch will not hold.
  • Zip replacement. Fitting a new zip means opening the suit and re-sealing the zip tape. That is a workshop job.
  • Large tears. Anything longer than a hand span, or a tear that crosses a seam.
  • Delaminated neoprene. Where the rubber layer has come away from the lining over a wide area.
A good rule: if the repair needs a sewing machine, send it out. If it needs glue and a patch, do it in the shop.

How to patch a neoprene tear

A clean tear is the easiest repair in the fleet. Keep a small kit in the shop: neoprene cement, patches cut from an old suit or neoprene offcuts, and a roller or a smooth bottle to press with.
  1. Clean the tear. Rinse with fresh water and let it dry completely. Glue does not stick to wet or salty neoprene.
  1. Line the tear up. Push the two edges together so they meet exactly. If the tear is jagged, trim any loose flaps first.
  1. Glue both edges. Spread a thin coat of neoprene cement on both sides of the tear. Use glue made for neoprene, not general-purpose glue.
  1. Wait until it is tacky. Let the glue dry until it is no longer wet to the touch. Do not press the edges together while the glue is still wet.
  1. Press the edges together. Push them firmly into place and hold them for a minute. Roll over the join to press out air.
  1. Patch the inside. For a tear in a high-stretch area, glue a patch over the inside of the repair. Cut the patch round, not square, so the corners cannot peel up.
  1. Leave it to cure. Do not put the suit back in the water until the repair has cured. Overnight is the usual rule.
A repair done this way is often stronger than the neoprene around it. A repair rushed while the glue is wet will peel open on the next dive.

How to fix a split seam

A seam splits when the stitching gives way or the glue line under it opens. You will see it first at the shoulders and the crotch, where the suit stretches most.
A small split in a glued seam can sometimes be re-glued in the shop if the stitching is still intact: clean the area, spread neoprene cement into the split, press it closed, and leave it to cure overnight.
If the stitching has gone, send the suit out. A blind-stitched seam is stitched with a curved needle that goes through one side of the neoprene but not all the way through. A shop without that machine cannot rebuild it, and a straight hand stitch through both layers turns a blind-stitched seam into a flatlock seam that lets water in.
When a suit comes back from a seam repair, turn it inside out, look at the seam, and pull it gently. The repair should hold without the neoprene tearing beside it.

Zips: care, common failures, and replacement

  • Rinse after every dive. Salt and sand are what kill zips. Rinse the zip in fresh water and run the slider up and down a few times while it is wet.
  • Keep sand out. Sand in the teeth is the usual cause of a stuck zip. Brush it out before you force anything.
  • Lubricate the teeth. A little zip wax or silicone lubricant on the teeth now and then keeps the slider moving. Do it when the zip is clean and dry.
  • Do not force a stuck zip. If the slider will not move, stop. Pull the suit material away from the zip so the teeth are not under tension, then work the slider back and forth gently. Forcing it bends the teeth, and bent teeth mean a new zip.
  • Check the slider. A zip that keeps popping open behind the slider usually has a worn slider, not worn teeth. A repair shop can fit a new slider without replacing the whole zip.
When teeth are missing or the zip tape is torn away from the suit, the zip has to be replaced. That is a workshop job. Compare the repair cost with the cost of a replacement suit before you send it, and retire the suit if the numbers are close.

Knee and seat wear

Knees and seats do not tear suddenly. They go thin first. Hold the neoprene up to the light: if you can see through the knee where the rest of the suit is solid, the knee is worn thin and will tear soon.
Patch thin knees before they tear. Glue a reinforcement patch over the worn area and let it cure overnight. It is a ten-minute job that adds months to a suit.

When a suit is beyond repair

Retire a suit when:
  • The neoprene is stiff or crumbling. Old neoprene loses its stretch and starts to crack. Glue will not stick to it and patches will not hold.
  • The neoprene has gone thin over a wide area. A suit that is thin across the chest or the knees no longer keeps a diver warm, even if it has no holes.
  • Several seams are splitting at once. One split seam is a repair. Three split seams is a suit at the end of its life.
  • The zip track is torn or teeth are missing in several places. A new zip costs a large part of what a new suit costs.
  • The suit no longer fits close. Neoprene stretches with age and heavy use. A loose suit lets in too much water, and no repair fixes that.
A suit that takes on too much water is a cold diver and a complaint. Retiring it on time is cheaper than the rental you lose.

What to check on a sample

Check these on the sample before you approve a fleet.
  • Turn the suit inside out and look at the seams. Even stitching, no skipped stitches, no loose thread ends. Pull a seam gently: it should hold without the neoprene tearing beside it.
  • Run the zip up and down several times. It should move smoothly with no catching. Check the teeth are even and the tape is firmly attached.
  • Check the knees and elbows. Look for reinforcement. On a rental suit, reinforced knees are worth asking for.
  • Feel the neoprene. It should be even in thickness across the suit, with no thin spots at the knees, seat, or shoulders.
  • Ask what happens if a seam or zip fails early. We stand behind the seams and zips. If a suit fails early, we replace it rather than argue about it.
A sample takes about 7 working days. Check the seams and the zip on the sample the same way you check a suit coming back from a dive, before you approve the full order.

The short version

Patch small tears in-house with neoprene cement and a round patch, and let them cure overnight. Send split seams and zip replacements to a repair shop. Rinse zips after every dive and never force a stuck slider. Patch thin knees before they tear, and retire a suit when the neoprene is stiff, thin, or splitting in several places.
If you are ordering a fleet and want a quote, tell us your water temperature, your thickness, and whether you want reinforced knees. We make to order, mixed sizes in one run, with your logo if you want it. MOQ is 50 pieces, samples take 7 working days, and production takes 25 days.

Frequently asked questions

What can I fix in the shop, and what should I send out? Small neoprene tears, worn knee patches, and zip care can be done in-house. Split seams and zip replacements need a repair shop, because they need the right machine.
How do I patch a neoprene tear? Clean the tear, glue both edges with neoprene cement, wait until the glue is tacky, press the edges together, patch the inside, and leave it to cure overnight before the suit goes back in the water.
What happens if a seam or zip fails early on a new suit? We stand behind the seams and zips. If a suit fails early, we replace it rather than argue about it.


Read next

Keep reading

Related guides for dive shops and brands.